MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV 24045DB Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 24045DB is an economic general purpose thermoplastic vulcanizate with good mechanical properties. This product is a high hardness, low density grade offered in Black for use in injection molded parts, extrusion s such as weather-stripping and blow-molded applications.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Fatigue Resistant; General Purpose: Good Adhesion; Good Moldability; Good Processability; Good Surface Finish; High Hardness; Low Density; Low Specific Gravity; Medium Heat Resistance; Resilient; Weather Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Interior Parts; Automotive Under the Hood; Blow Molding Applications; Grommets; Industrial Applications; Plugs, Profiles; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion; Extrusion Blow Molding; Blow Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccISO 1183
Viscosity 310 cP
@Shear Rate 206 1/s,
Temperature 200 °C
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50
@Time 5.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 2900 psiAcross Flow; ISO 37
Tensile Stress at Strain 1740 psi
@Strain 100 %
Across Flow; ISO 37
Elongation at Break 700 %Across Flow; ISO 37
Tear Strength 750 pliMethod Ba, Angle (Unnicked), Across Flow; ISO 34-1
Compression Set 75 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Processing Temperature 369 - 428 °FInjection, Melt
Rear Barrel Temperature 356 - 419 °FInjection
Middle Barrel Temperature 356 - 419 °FInjection
Front Barrel Temperature 356 - 419 °FInjection
Nozzle Temperature 369 - 428 °FInjection
Zone 1 356 - 392 °FExtrusion
Zone 2 356 - 410 °FExtrusion
Zone 3 356 - 410 °FExtrusion
Zone 4 356 - 410 °FExtrusion
Die Temperature 383 - 419 °FExtrusion
Melt Temperature 383 - 419 °FExtrusion
Mold Temperature 50.0 - 131 °FInjection
Drying Temperature 180 °F
Dry Time 3.00 hour
Back Pressure 14.5 - 145 psiInjection
Screw Speed 100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Griltech Griltex® D 1666A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Titanium Ti-8Mo-8V-2Fe-3Al, ST 785°C, Quenched
Special Metals NILO® Alloy 36 Low-Expansion Alloy
EN SPH235 High Manganese Pressure Vessel Carbon Steel

PTEKNQ1182 / 237673

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.