MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Röchling Glastherm® HT 200 Heat Insulation component
Categories: Polymer; Thermoset

Material Notes: Glastherm® HT 200 is a heat insulation system with a high level of stability which is suitable for processes with a working temperature of up to 200°C (392°F). Glastherm® HT 200 was developed specially for plastic and zinc die-casting molds. It has good thermal insulation, enabling rapid die heating-up processes and therefore rapid start-up of the machines. Glastherm® HT 200 is free of asbestos and can be easily cut and adapted with standard metal tools.
  • Maximum continuous operation temperature: 200°C (392°F)
  • High compressive strength: 230 MPa (at 200°C)
  • Good thermal insulation

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.90 g/ccISO 1183
Water Absorption <= 0.10 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 200 MPaISO 178
Compressive Strength 230 MPa
@Temperature 200 °C
20x20x20 mm; ISO 604
 320 MPa
@Temperature 23.0 °C
Perpendicular, 20x20x20 mm; ISO 604
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°CParallel
Thermal Conductivity 0.300 W/m-KPerpendicular
Maximum Service Temperature, Air 392 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROCH9119 / 232822

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.