MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Polyram PlusTek PA310G8BK10 Nylon 6.6 for injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Heat stabilized, 40% Glass fiber reinforced Nylon 6.6 for injection molding applications. Approved and listed by NSF/ANSI 61 International.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccISO 1183
Moisture Absorption at Equilibrium 1.5 %50% RH; ISO 62
Water Absorption at Saturation 4.7 %ISO 62
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 122
Tensile Strength, Yield 210 MPaISO 527
Elongation at Break 2.0 %ISO 527
Tensile Modulus 12165 MPaISO 527
Flexural Strength 320 MPaISO 178
Flexural Modulus 13500 MPaISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature -30.0 °C
ISO 180
 13.0 kJ/m²
@Temperature 23.0 °C
ISO 180
Charpy Impact Unnotched 75.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 90.0 kJ/m²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 13.5 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 90.0 kV/mmIEC 60250
 
Thermal PropertiesOriginal ValueComments
Melting Point 256 °CISO 11357
Maximum Service Temperature, Air 120 °CContinuous use
 240 °CShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 260 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 240 °CISO 75
Flammability, UL94 HB
@Thickness 3.00 mm
Flame Spread 10 mm/minFMVSS302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyram PlusTek PA7001G7BK11 Nylon 66, 35% Glass Fiber Reinforced, Heat and UV Stabilized, Hydrolysis Resistant
Polyram PlusTek PA301G7 Nylon 6.6, Heat Stabilized 35% Glass Fiber
Polyram PlusTek RA300G7 Nylon 6.6 for Injection Molding, 35% Glass Fiber Reinforced, Heat Stabilized
Polyram PlusTek PA7800G33 Nylon 6.6 for Injection Molding, 33% Glass Fiber Reinforced, Heat Stabilized, Impact Modified

PPOLYR831 / 126630

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.