MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nordel® IP 4770R Heat Resistant Peroxide Compound
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nordel® IP 4770R is a high molecular weight semicrystalline grade and offers fast cure rates and high states of cure with standard sulfur cure systems. It offers high green strength and high extensibility. It is designed for extruded applications such as profiles and hose. It is also suitable for molded goods. This grade is available in rod form for improved mixing speed and throughput.

Information provided by manufacturer.

Key Words: 0072A38-11
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.064 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74Vulcanizate, Press cured, TC95 +3min at 180°C
Tensile Strength, Ultimate 26.1 MPaVulcanizate, Press cured, TC95 +3min at 180°C
Elongation at Break 266 %Vulcanizate, Press cured, TC95 +3min at 180°C
100% Modulus 0.00560 GPa
@Strain 100 %
Vulcanizate, Press cured, TC95 +3min at 180°C
200% Modulus 0.0170 GPa
@Strain 200 %
Vulcanizate, Press cured, TC95 +3min at 180°C
Tear Strength 30.6 kN/mDie C, Vulcanizate, Press cured, TC95 +3min at 180°C
Compression Set 61 %
@Temperature 125 °C
Pellets cured MDR t'95 + 15 min, 70 hr; Method B
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -28.0 °CTemperature Retraction, TR-10
 
Descriptive Properties
Formulation as Tested10Paraffinic Oil
 100Nordel® IP 4770R
 50N-550 Black
 7DCP-40% Active

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nordel® IP 5565 General Purpose Molding
Dow Nordel® NDR 4820P EPDM Hydrocarbon Rubber
Dow AFFINITY™ VP 8770 Polyolefin Plastomer
Dow Nordel® IP 4640 Molded Golf Grips
Dow Nordel® IP 4640 Molded Brake Cup

PDVG40 / 34160

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.