MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Antilux® 111 Wax
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Wax to protect rubber articles against cracking caused by ozone and weathering influences.

Use: Antilux 111, with its reduced solubility migrates to the surface of the vulcanizates where it forms a complete protective film which remains stable at temperatures up to about 50 °C. The formation of the film takes place at a slow rate. The protective film shows an excellent stability against dynamic stress. Antilux 111 provides a most effective long term protection.

Application: Tires and conveyor belts as well as technical rubber articles of all kinds which are used at higher service temperatures. Antilux 111 meets test specifications at ozone chamber temperatures of about 50 °C. The protection may be extended by means of blending with lower melting Antilux grades.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/cc
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 50.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 36.5 Month
@Temperature <=35.0 °C
 
Descriptive Properties
Appearancelight green flakes
Specifications64-67°CCongealing point, ISO 2207

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8257 / 208650

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.