MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
348 Stainless Steel, annealed, strip
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Niobium plus Tantalum is ten times the minimum carbon content

Key Words: UNS S34800, ASME SA182, ASME SA213, ASME SA240, ASME SA249, ASME SA312, ASME SA358, ASME SA376, ASME SA403, ASME SA409, ASME SA479, ASTM A167, ASTM A182, ASTM A213, ASTM A240, ASTM A249, ASTM A269, ASTM A276, ASTM A312, ASTM A314, ASTM A358, ASTM A376, ASTM A403, ASTM A479, ASTM A580, ASTM A632, B.S. 347 S 17, B.S. 347 S 18, B.S. 347 S 40, B.S. 2 S. 130 (U.K), B.S. S. 525, B.S. S. 527, FED QQ-S-766, MIL SPEC MIL-S-23195, MIL SPEC MIL-S-23196, SAE J405 (30348), DIN 1.4546
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 147Converted from Rockwell B hardness.
Hardness, Knoop 164Converted from Rockwell B hardness.
Hardness, Rockwell B 85
Hardness, Vickers 169Converted from Rockwell B hardness
Tensile Strength, Ultimate 655 MPa
Tensile Strength, Yield 275 MPa
@Strain 0.2 %
Elongation at Break 45 %in 50 mm
Modulus of Elasticity 195 GPa
Poissons Ratio 0.27
Shear Modulus 77.0 GPa
Izod Impact 120 - 160 J
Charpy Impact 160 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000791 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.3 µm/m-°C
@Temperature 0.000 - 100 °C
 17.8 µm/m-°C
@Temperature 0.000 - 260 °C
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.3 W/m-K
@Temperature 100 °C
 21.5 W/m-K
@Temperature 500 °C
Melting Point 1400 - 1425 °C
Solidus 1400 °C
Liquidus 1425 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 19 %
Cobalt, Co 0.20 %
Iron, Fe 66 %
Manganese, Mn <= 2.0 %
Nb + Ta 0.80 %
Nickel, Ni 11 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %
Tantalum, Ta 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
347 Stainless Steel, annealed, strip
321 Stainless Steel, annealed strip
AISI Type 316N Stainless Steel, annealed sheet
AISI Type 317L Stainless Steel, annealed sheet
348 Stainless Steel, annealed, sheet

MQ348AN / 12888

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.