(Viewing data as-entered.
Click here
to return)
Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue Stick
Categories:
Polymer
;
Adhesive
;
Thermoplastic
;
Nylon (Polyamide PA)
Material Notes:
Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue Stick
Medium performance. Oil resistance for wood, fabric and other porous substrates primarily in woodworking assembly operation.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Viscosity
11500
cP
@Temperature 177 °C
Typical
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
196
°F
Minimum Service Temperature, Air
-40.0
°F
Processing Properties
Original Value
Comments
Pot Life
5.0
-
30
sec
Open Time
Descriptive Properties
Color
Clear Amber
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Valley Adhesives EM-422 High Temperature Application Glue Stick
Parson Adhesives PARLITE® 4760 UV Glue and UV Adhesive for Electronic Assembly
Lord Adhesives 360 Sag-Resistant, High-Performance, 5 min Epoxy Adhesive
Chemical Concepts H2O Glue® Aquabonder Underwater Adhesive
Bostik 6332 Quick Setup EVA Glue Stick
PBOST05 / 27564
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.