MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay DERMALCARE® MAP L 210 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: High purity Monoalkyl Phosphate based off patented Rhodia process. Upon neutralization, MAP L-210 is extremely mild to the skin and imparts a soft elegant skin feel. Provides a dense, creamy lather to formulated products.

Chemical Name: COMPLEX ORGANIC PHOSPHATE ESTER, FREE ACID

CAS: 39464-66-9, 4536-30-5, 7664-38-2

Available in: Asia Pacific, Europe, Latin America and North America

Applications: DERMALCARE MAP-L-210 is a high purity Laureth-1 Phosphate ester in the free acid form. Typically used in facial and skin cleanser applications, Dermalcare MAP-L 210 can be neutralized with any common base to yield ultra-mild surfactants that produce a luxurious, creamy lather. In formulated systems, Dermalcare MAP-L-210 imparts an elegant, soft feel to skin.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH <= 2.510% Solution; RP-0402
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 176 - 184(100% Basis); RP-0427
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0
@Temperature 50.0 °C
RP-0138
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 1.0 %RP-0327
 
Descriptive Properties
AppearanceWhite to pale yellow, low MP soft solidRP-0064
CompositionFree Acid (As H3PO4)<7%, RP-0427
 Nonionics<6%, RP-0966

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD108 / 137339

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.