MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ineos TUB121B High density bimodal polyethylene copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: TUB121B is a black high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, industrial, and mining pipe. It is listed by the Plastics Pipe Institute (PPI TR-4, as both PE 4710 and PE 100) and is certified to NSF/ANSI Standard 14, NSF/ANSI Standard 61, CSA B137.1 and CSA B137.4.

Information provided by INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9485 g/ccNatural; ASTM D4883
 0.959 g/ccBlack; ASTM D4883
Environmental Stress Crack Resistance >= 5000 hourCondition C; ASTM D1693
Carbon Black Loading 2.3 %ASTM D1603
Melt Flow 0.30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
 8.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
PENT >= 10000 hourASTM F1473
Hardness, Shore D 66ASTM D2240
Tensile Strength at Break 31.7 MPa2 in/min; ASTM D638
Tensile Strength, Yield 25.0 MPa2 in/min.; ASTM D638
Elongation at Break >= 600 %2 in/min; ASTM D638
2% Secant Modulus 896 MPaMethod 1; ASTM D790
Izod Impact, Notched (ISO) 0.490 kJ/m²ASTM D256
Hydrostatic Design Basis >= 10.0 MPaISO 9080
 6.90 MPa
@Temperature 60.0 °C
ASTM D2837
 11.0 MPa
@Temperature 23.0 °C
ASTM D2837
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 126 °CASTM D1525
Brittleness Temperature <= -118 °CASTM D746
 
Descriptive Properties
Cell Classification445576CASTM D3350
Oxidative Resistance ClassificationCC3ASTM D3350
Thermal Stability (°C)>220ASTM D2513/ ASTM D3350

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINEOS870 / 291476

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.