MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics AL 995™ Mac-A995W Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: High purity alumina ceramic of 99.5% Al2O3 content. Its purity, chemical resistance and high temperature capabilities prove invaluable for semiconductor processing applications.

Prime Features:

  • Electrically and dimensionally stable at high temperatures
  • Low particle generation
  • Dense, non-porous and vacuum tight
  • Excellent dielectric properties
  • Accepts moly-manganese metallizing for high temperature brazing of vacuum tight assemblies
  • Excellent chemical and abrasion resistance
Typical applications:
  • Wafer processing and handling devices
  • Components for semiconductor process ambers, spluttering targets, fixtures, etc. Laser devices for wide range of industrial, medical and defence duties
  • Power tubes for klystron and x-ray equipment
  • Flow meters and pressure sensors
Production Capabilities:
  • Isostatic and dry pressing, green machining
  • CNC grinding and lapping to very tight tolerances
  • Metallising of components
  • High temperature brazing of assemblies
  • Prototype, batch and volume production

Information provided by Morgan Advanced Materials

Key Words: Mac-A995W
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 3.86 g/cc
Open Porosity 0.00 %fully dense, % nominal, apparent
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell HR45N 81
Flexural Strength 310 MPa
Compressive Strength 2070 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.20e+9 ohm-cm
@Temperature 500 °C
 2.00e+11 ohm-cm
@Temperature 300 °C
 >= 1.00e+14 ohm-cm
@Temperature 25.0 °C
Dielectric Constant 9.3
@Frequency 1e+9 Hz,
Temperature 25.0 °C
 9.37
@Frequency 8.50e+9 Hz,
Temperature 25.0 °C
 9.58
@Frequency 1e+7 Hz,
Temperature 25.0 °C
 9.61
@Frequency 8.50e+9 Hz,
Temperature 300 °C
 9.82
@Frequency 8.50e+9 Hz,
Temperature 500 °C
 9.92
@Frequency 1e+7 Hz,
Temperature 300 °C
 10.2
@Frequency 1e+7 Hz,
Temperature 500 °C
Dielectric Strength 800 V/mil
Dissipation Factor 0.000030
@Frequency 1e+7 Hz,
Temperature 25.0 °C
 0.000090
@Frequency 8.50e+9 Hz,
Temperature 25.0 °C
 0.000090
@Frequency 1e+7 Hz,
Temperature 300 °C
tan d
 0.00014
@Frequency 8.50e+9 Hz,
Temperature 300 °C
 0.00014
@Frequency 1e+9 Hz,
Temperature 25.0 °C
 0.00025
@Frequency 8.50e+9 Hz,
Temperature 500 °C
 0.00040
@Frequency 1e+7 Hz,
Temperature 500 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.90 µm/m-°C
@Temperature 25.0 - 200 °C
 7.80 µm/m-°C
@Temperature 200 - 400 °C
 8.30 µm/m-°C
@Temperature 400 - 600 °C
 9.00 µm/m-°C
@Temperature 600 - 800 °C
 9.40 µm/m-°C
@Temperature 800 - 1000 °C
Thermal Conductivity 29.3 W/m-K
Maximum Service Temperature, Air 1725 °Cno load
 
Component Elements PropertiesOriginal ValueComments
Al2O3 99.5 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Morgan Advanced Ceramics AL-300™ 97-99% Alumina
Hydrogenated Nitrile Rubber (HNBR)
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3)
CeramTec B 40 Alumina, 99.1%

CMORF5026 / 200264

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.