MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Melos Mecoline I RDX 5210 F Radiation cross-linkable, flame retardant insulation compound
Categories: Polymer; Thermoplastic

Material Notes: Radiation cross-linkable, flame retardant insulation compound.

Compound class: Sheathing

Compound category: RDX

Flame retardant: ATH

Standards: Chrysler MS 9502A; MS 9502B; LV 112 Class C; ISO 6722 Class C; SAE J-1128 TXL, GXL and SXL; LV 112 Class D; ISO 6722 Class D; Ford ES-AU5T-1A348-AA

Typical applications: A high performance radiation cross-linkable compound, offering excellent mechanical and electrical properties.

Features: Flame retardant; Low smoke; High temperature resistant; Oil resistant; Abrasion resistant

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccpressed plaques; DIN EN ISO 1183-1A
Melt Flow 0.60 g/10 min
@Load 21.6 kg,
Temperature 190 °C
DIN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 54pressed plaques; DIN ISO 7619-1
Tensile Strength >= 10.0 MPaextruded tapes; IEC 60811-501
 20.0 MPacross-linked plaques or tapes, 120kGy; IEC 60811-501
 >= 10.5 MPa
@Temperature 180 °C,
Time 864000 sec
extruded tapes, After ageing in air oven; MS 9502B
 >= 11.5 MPa
@Temperature 150 °C,
Time 1.08e+7 sec
extruded tapes, After ageing in air oven; MS 9502B
Elongation at Break 250 %cross-linked plaques or tapes, 120kGy; IEC 60811-501
 >= 600 %extruded tapes; IEC 60811-501
Tear Strength 70.1 kN/mAfter cross-linking, (120kGy); MS 9502B
Abrasion 1900pressed plaques; MS 9502B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 205 - 215 °CTool
 230 °CMaximum mass temperature
Zone 1 160 - 170 °C
Zone 2 180 - 190 °C
Zone 3 190 - 200 °C
Zone 4 190 - 200 °C
Zone 5 190 - 200 °C
Adapter Temperature 190 - 200 °C
Head Temperature 190 - 200 °C
Drying Temperature 60.0 - 70.0 °C
Dry Time 4.00 - 6.00 hour
 
Descriptive Properties
Main burning properties5 sec45 degree flame resistance test, MS 9502 B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMELOS025 / 296132

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.