MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco ISO 68 Red Chain Bar Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Red Chain Bar Oils are very tacky, tough, lubricants made from special high viscosity base oils having the desired flow and pumpability properties to assure adequate lubrication over a wide range of ambient temperatures.

Chevron Red Chain Bar Oils are manufactured to meet the needs of the forest products industry under the most adverse operating conditions. To a logger, chainsaw lubrication is one of the most demanding requirements for efficient chainsaw performance and operation. Chevron Red Chain Bar Oils were designed to meet this demand with economy in mind.

There are four grades of Chevron Red Chain Bar Oils to meet any ambient temperature requirements.

ISO 68 is recommended for winter conditions when temperatures are consistently below 0°C (32°F).

ISO 100 is the ideal grade for cool weather conditions of 0-15°C (32-60°F) to assure a proper flow from either hand operated or automatic chain oilers.

ISO 150 is a good choice for all-season use in mild climates and provides excellent wear protection under hot weather operating conditions.

ISO 220 is often preferred by forest industry professionals during the summer season due to its outstanding lubricating and film retention properties. The higher viscosity of the ISO 220 grade, in combination with wear protection additives, provides the extra level of protection needed in high performance professional saws.

Applications

Chevron Red Chain Bar Oils are recommended for use in all types of chain saws using either hand-operated or automatic chain oilers to lubricate the chain, bar, and sprocket.

Other possible uses include chain drives on straddle lift lumber carriers and motorcycle chains, as well as lawnmowers and farm equipment.

Key Words: CPS Number: 225156; MSDS Number: 6804
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 27.7 °
Saybolt Viscosity at 100°F 335 SUS
Kinematic Viscosity at 40°C (104°F) 65 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -30.0 °CASTM D97
Flash Point 200 °CASTM D92
 
Descriptive Properties
Pall Filterability, Wet aged, mL to 25 psi>3500

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco FM ISO 68 Lubricating Oil
ChevronTexaco TEGRA® ISO 68 Synthetic Compressor Oil

WCHEV168 / 74783

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.