MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum AL 409HP™ Ferritic Stainless Steel, UNS S40930
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Type 409 ferritic stainless steel was introduced by Allegheny Ludlum in 1961 to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon automotive exhaust systems in comparison to carbon steel. They alloy wad designated MF-1 indicating its end use: automotive mufflers. The good fabricability of this alloy, combined with its basic corrosion resistance and economy have significantly broadened the utility of Type 409.

Since its introduction, the Type 409 alloy has been widely used in automotive exhaust systems for manifolds, exhaust pipes, catalytic converters, mufflers, tail pipes and other components. Type 409 stainless steel sheet has also found many other applications such as in culverts, home heating systems, automotive thermostats and fuel filters, electrical transformer cases, caskets, heat exchanger tubing, and various farm equipment components. Plate has been used as blades and vanes in standby power generation turbines and as jet engine sound-deadening devices at airports.

The performance of Type 409 ferritic stainless steel in most applications has been excellent. However, some industry application have resulted in intergranular corrosion of weld heat-affected zones. The result of Allegheny Ludlum's research to investigate and redefine the balance of stabilizing elements is the AL 409HP stainless steel amounts of titanium and columbium which provide resistance to sensitization and intergranular corrosion which might occur in the heat affected zones of welds or in base metal following other thermal exposures. A low incidence of titanium nitride surface imperfections is also a characteristic of this alloy. The balance of stabilizing elements is designed to optimize weldability without need for post-weld annealing to restore ductility. Formability and toughness are also improved in comparison to the standard Type 409 alloy.

This AL 409HP alloy is a proprietary stainless steel composition. Like all Type 409 alloys, the AL 409HP stainless steel contains nominally 11 percent chromium for greatly enhanced corrosion resistance in comparison to carbon steel. It is an excellent choice for all automotive exhaust system applications where 11 percent chromium provides sufficient resistance to oxidation and corrosion. Hot end exhaust applications may require an 18 percent chromium alloy.

Information provided by Allegheny Ludlum

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.76 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 71typical annealed
Tensile Strength, Ultimate 434 MPatypical annealed
Tensile Strength, Yield 241 MPa
@Strain 0.2 %
typical annealed
Elongation at Break 33 %
@Thickness 50.8 mm
typical anneal
Modulus of Elasticity 200 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000600 ohm-cm
Curie Temperature 732 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.52 µm/m-°C
@Temperature 20.0 - 100 °C
 11.11 µm/m-°C
@Temperature 20.0 - 260 °C
 11.88 µm/m-°C
@Temperature 20.0 - 482 °C
Specific Heat Capacity 0.477 J/g-°C
Thermal Conductivity 25.0 W/m-K
Maximum Service Temperature, Air 760 °CSignificant oxidation resistance to this temp.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.010 %
Chromium, Cr 11 %
Iron, Fe 88 %as balance
Manganese, Mn 0.30 %
Nickel, Ni 0.25 %
Niobium, Nb (Columbium, Cb) 0.15 %
Nitrogen, N 0.012 %
Phosphorus, P 0.023 %
Silicon, Si 0.41 %
Sulfur, S 0.0010 %
Titanium, Ti 0.17 %(Ti + Nb) = 0.08 + 8 * (C+N) min.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel 12 SR™ Ferritic Stainless steel
ATI Allvac® Vasco® Greek Ascoloy Specialty Steel, Heat Treatment: 871°C (1600°F) + Age
403 Stainless Steel, annealed, bar
430 Stainless Steel annealed bar
AISI 1010 Steel, cold drawn

NL409 / 17888

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.