MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® G1740 M (SEP) Star Polymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G1740 M is a clear, star polymer based on styrene and ethylene/propylene with a polystyrene content of 6%. It is supplied from North America in the physical form identified:
Kraton G1740 MU - supplied as a powder.

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton G1740 M is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.

Applications: Compounding and Personal Hygiene; Adhesives, Sealant and Coatings; Packaging and Polymod; and Personal Care

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.70 %KM 04
Kinematic Viscosity at 100°C (212°F) 13.8 - 16.2 cSt1.23%, ENJ411; BAM 1201
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.03-0.2%, KM 08
 Polystyrene4.5-6.8%, Measured on the polymer before hydrogenation, KM 03
 Total Extractables<3.0%, KM 05

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® FG1901 G (SEBS) grafted with MA
Kraton® G1641 H (SEBS) Linear Triblock Copolymer
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Kraton® G1651 E (SEBS) Linear Triblock Copolymer

PKRA9907 / 132806

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.