MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger ENSITEP® PBT Polybutylene Terephthalate - Extruded Products  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Extrusion Grade

Material Notes: ENSITEP BT is an unreinforced thermoplastic polyester derived from polybutylene terephthalate. Its excellent wear and impact resistance, low coefficient of friction, high flexural modulus, and superior dimensional stability make it a versatile material for designing mechanical and electro-mechanical parts. Because ENSITEP BT has no centerline porosity, the possibility of fluid absorption and leakage is virtually eliminated.

Uses: ENSITEP's superior wear resistance and lack of centerline porosity give it an advantage over other materials for applications involving solvents, chemicals, and food products. ENSITEP is also used in water purification systems, printing equipment, textile components, food-handling equipment, and valves.

Ensitep grades have been replaced by Tecapet

Information supplied by Ensinger, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccASTM D792
Water Absorption 0.080 %24 hrs.; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 72ASTM D785
Tensile Strength at Break 59.9 MPaASTM D638
Elongation at Break 300 %ASTM D638
Modulus of Elasticity 2.86 GPaASTM D638
Flexural Yield Strength 82.7 MPaASTM D790
Flexural Modulus 2.28 GPaASTM D790
Poissons Ratio 0.38Calculated
Shear Modulus 1.04 GPa
Izod Impact, Notched 0.800 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.2
@Frequency 100 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm
@Thickness 3.17 mm
short term; ASTM D149
Dissipation Factor 0.0010
@Frequency 100 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 83.5 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 1.30 J/g-°C
Thermal Conductivity 1.46 BTU-in/hr-ft²-°FASTM C177
Melting Point 254 °C
Deflection Temperature at 0.46 MPa (66 psi) 154 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °CASTM D648
Flammability, UL94 HB

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES HiFill® PBT E
Polyplastics Duranex® 700FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, High Viscosity
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
Kolon SPESIN® KP270 General Purpose PBT Base Resin
Eurotec® Tecodur® PB30 NL PBT, unfilled, natural, high viscosity, extrusion grade

PENS21 / 35979

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.