MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Nouryon Duomeen OL Di-amine, oleyl
Categories: Other Engineering Material

Material Notes: Duomeen OL

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.810 g/cc
@Temperature 70.0 °C
 0.817 g/cc
@Temperature 60.0 °C
 0.831 g/cc
@Temperature 40.0 °C
 0.843 g/cc
@Temperature 25.0 °C
Viscosity 14 cP
@Temperature 35.0 °C
 17 cP
@Temperature 30.0 °C
 19 cP
@Temperature 25.0 °C
Vapor Pressure 0.000300 bar
@Temperature 18.0 °C
 0.00100 bar
@Temperature 43.0 °C
 0.00220 bar
@Temperature 65.0 °C
 0.00520 bar
@Temperature 93.0 °C
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.606 BTU/lb-°F
@Temperature 37.8 °C
 0.617 BTU/lb-°F
@Temperature 60.0 °C
 0.623 BTU/lb-°F
@Temperature 71.1 °C
 0.641 BTU/lb-°F
@Temperature 93.3 °C
Melting Point 12.0 °C
Boiling Point >= 300 °C
@Pressure 0.101325 MPa
Pour Point 18.0 °C
Flash Point >= 150 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 0.00 - 5.0
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 1.0 %
 
Descriptive Properties
Amine number320-350 mg KOH/g
AppearanceLiquid
Cloud point20°C
Content= 70 g I2/100 gIodine value
 = 89 %Apparent diamine activity
 160-175 g/eqNeutralization equivalent
 43-52%(Mw=161), Primary Amine
 43-52%(Mw=161), Secondary Amine
Equivalent mass160-175
HLB15.2Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY494 / 286017

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.