MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wacker Silres® REN 80 Heat Resistant Silicone Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: SILRES® REN 80 is a methyl phenyl group containing silicone resin solution in xylene.

Properties: SILRES® REN 80 is typically used in heat resistant coatings. It combines outstanding heat resistance and weatherability. With proper coating formulation, thermal stability up to 650°C (1200°F) can be achieved in combination with suitable temperature stable pigments and fillers.

Special features:

  • very good balance of flexibility, hardness, heat resistance and curing speed
  • high viscosity
  • medium hardness
  • coatings dry tack-free at room temperature
  • good compatibility with organic resins (but preferably used as a sole binder)
  • excellent hydrophobicity and corrosion-protection
Application: SILRES® REN 80 is suitable for all kinds of heat resistant paints. It is an excellent choice for (anticorrosion) coatings on mufflers, exhaust systems, engine parts, boilers, furnaces, ovens and oven inserts, chimneys, barbeques and electric and gas heaters, incinerators. At temperatures above 250°C (480°F) the organic groups of silicone resins start to degrade. After all the organic parts of the silicone resin have been pyrolytically decomposed, the product that remains moves to an inorganic stoichiometric composition of (SiO2)n. It is this layer which firmly binds pigments and fillers to the coated substrate.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccDIN 51757
Solids Content 80 - 84 %
@Treatment Temp. 200 °C,
Time 3600 sec
Viscosity 2000 cPdynamic; DIN 53019
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 650 °C
Flash Point 25.0 °CDIN 51755
Ignition Temperature 485 °CDIN 51794
 
Descriptive Properties
Appearanceclear, colorless to slightly yellow solution

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CMT Materials REN Shape® 440 Tooling Board, Modeling Board, Adhesive Products
Wacker Silres® REN 60 Heat Resistant Silicone Coating
CMT Materials REN Shape® 550 Tooling Board, Modeling Board, Adhesive Products
CMT Materials REN Shape® 5025 Tooling Board, Modeling Board, Adhesive Products
CMT Materials REN Shape® 5008 Vacuum Forming Tooling Board

PWACK9585 / 205114

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.