MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® G-101 Fluoroelastomer Plasticizer with DAI-EL® G-704 Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-101 is an ultra low molecular weight fluoroelastomer. At room temperature it is an opaque paste. At temperatures above 70°C (158 °F) it becomes a transparent, viscous fluid. DAI-EL® G-101 is not crosslinkable but is used as a plasticizer in other fluoroelastomers.

Typical Applications: Additive for other DAI-EL® fluoroelastomers. Mechanical property data shows effect of G-101 plasticizer on DAI-EL® G-704 Fluoroelastomer.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.76 - 1.77 g/ccDAI-EL® G-101
Viscosity 50 cP
@Temperature 60.0 °C
DAI-EL® G-101
Molecular Weight 3000 g/molDAI-EL® G-101
Evaporation Loss 2.0 %
@Temperature 200 °C,
Time 7200 sec
DAI-EL® G-101
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55G-704, 20 PHR G101 added
 61G-704, 0 PHR G101 added
 58
@Treatment Temp. 230 °C,
Time 86400 sec
After Air Aging, G-704, 20 PHR G101 added
 64
@Treatment Temp. 230 °C,
Time 86400 sec
After Air Aging, G-704, 0 PHR G101 added
Tensile Strength at Break 7.80 MPaG-704, 20 PHR G101 added
 10.3 MPaG-704, 0 PHR G101 added
 8.74 MPa
@Treatment Temp. 230 °C,
Time 86400 sec
After Air Aging, G-704, 20 PHR G101 added
 10.8 MPa
@Treatment Temp. 230 °C,
Time 86400 sec
After Air Aging, G-704, 0 PHR G101 added
Elongation at Break 290 %G-704, 0 PHR G101 added
 370 %G-704, 20 PHR G101 added
 299 %
@Treatment Temp. 230 °C,
Time 86400 sec
After Air Aging, G-704, 0 PHR G101 added
 381 %
@Treatment Temp. 230 °C,
Time 86400 sec
After Air Aging, G-704, 20 PHR G101 added
100% Modulus 0.900 MPa
@Strain 100 %
G-704, 20 PHR G101 added
 1.40 MPa
@Strain 100 %
G-704, 0 PHR G101 added
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.80e+12 ohm-cmDAI-EL® G-101
Dissipation Factor 0.0026
@Frequency 100 Hz
DAI-EL® G-101
 0.080
@Frequency 100000 Hz
DAI-EL® G-101
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.360 BTU/lb-°F
@Temperature 80.0 °C
DAI-EL® G-101
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.37DAI-EL® G-101
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
@Temperature 170 °C
Press cure, G-704
 24.0 hour
@Temperature 200 °C
Oven cure, G-704
 
Descriptive Properties
Test Formula100 phrRaw rubber (DAI-EL® G-704)
 3 phrMagnesium oxide
 6 phrCalcium hydroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDAIJ9872f / 210146

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.