MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cabot CABELEC® CA6114 HDPE, Conductive Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product highlights: CABELEC CA6114 electrically conductive compound is made from conductive carbon black dispersed in a modified high-density polyethylene resin. Its electrical and mechanical properties are not impacted by normal atmospheric conditions.

Key applications: CABELEC CA6114 conductive compound is used for injection molding applications. It is suitable for product handling applications where it is desirable to mitigate the hazard of electrostatic discharge, such as in automotive fuel systems or the handling and packaging of explosive powders and liquids, pigments or electronic components.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.065 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.025 - 0.035 cm/cmon UL94 bars; ASTM D955
Melt Flow 1.0 g/10 min
@Load 190 kg,
Temperature 5.00 °C
ISO 1133
 5.0 g/10 min
@Load 190 kg,
Temperature 10.0 °C
ISO 1133
 16 g/10 min
@Load 190 kg,
Temperature 21.6 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61
@Time 15.0 sec
ISO 868
Tensile Strength at Break 18.0 MPaISO 527
Tensile Strength, Yield 22.0 MPaISO 527
Elongation at Break 147 %ISO 527
Elongation at Yield 19 %ISO 527
Flexural Strength 23.0 MPaISO 178
Flexural Modulus 744 MPaISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²ISO 180A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 100 ohm-cminjection molded parts; IEC 61340-2-3
Surface Resistance <= 1.00e+13 ohminjection molded parts; IEC 61340-2-3
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °CISO 75/2
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °CISO 75/2
Vicat Softening Point 119 °C
@Load 1.02 kg
ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 °Cbarrel
Nozzle Temperature 230 °C
Mold Temperature 35.0 - 45.0 °C
Drying Temperature 90.0 °C
Dry Time 2.00 - 3.00 hour
Screw Speed 50 - 60 rpm
 
Descriptive Properties
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT045 / 315780

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.