MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound 9X06483 Polyamide 46 (Nylon 46)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46)

Material Notes: LNP LUBRICOMP 9X06483 compound is based on a Nylon 4/6 resin containing PTFE. Added features of this grade include: Wear Resistant, Heat Stabilized.

Features: Wear resistant,Heat Stabilized

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.28 g/ccISO 1183
 1.29 g/ccASTM D792
Moisture Absorption 0.0500 %Injection Molding
 1.80 %23°C/50% RH/24 hrs; ASTM D570
 2.70 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.010 - 0.030 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 74.0 MPa5 mm/min; ASTM D638
 76.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 78.0 MPa5 mm/min; ISO 527
 80.0 MPa5 mm/min; ASTM D638
Elongation at Break 5.9 %5 mm/min; ASTM D638
 6.6 %5 mm/min; ISO 527
Elongation at Yield 5.8 %5 mm/min; ASTM D638
 6.5 %5 mm/min; ISO 527
Tensile Modulus 3000 MPa1 mm/min; ISO 527
 3130 MPa5 mm/min; ASTM D638
Flexural Strength 101 MPa2 mm/min; ISO 178
Flexural Modulus 2800 MPa2 mm/min; ISO 178
 2960 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 52.0 JASTM D256
Izod Impact, Unnotched 924 J/mASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 56.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 3.00 JASTM D3763
Coefficient of Friction, Dynamic 0.32ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.32ASTM D3702 Modified: Manual
K (wear) Factor 11.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 93.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 276 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 283 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 151 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 300 - 310 °C
Zone 3 310 - 320 °C
Melt Temperature 310 - 320 °CInjection Molding
Mold Temperature 80.0 - 120 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 40.0 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80658 / 288605

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.