MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Hostaform® C 27021 AST POM, Specialty
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Chemical abbreviation according to ISO 1043-1: POM

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Water Absorption at Saturation 0.70 %ISO 62
Linear Mold Shrinkage, Flow 0.019 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.018 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 63.0 MPa50mm/min; ISO 527-2/1A
Elongation at Break 17 %50mm/min; ISO 527-2/1A
Elongation at Yield 8.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 2800 MPa1mm/min; ISO 527-2/1A
Flexural Modulus 2700 MPaISO 178
Charpy Impact Unnotched 120 kJ/m²ISO 179/1eU
 120 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²ISO 179/1eA
 5.50 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2400 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 1300 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 110 µm/m-°CISO 11359-2
Melting Point 166 °CISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 100 °CISO 75-1, -2
Vicat Softening Point 150 °CB50 (50°C/h 50N); ISO 306
 
Descriptive Properties
Injection moldingYes
Melt volume rate (MVR), cm³/10min24.5
MVR test load, kg2.16
MVR test temperature, °C190
Processing conditions acc. ISO9988

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hostaform® C 27021 AS POM, Specialty
Celanese Hostaform® C 27021 POM, Unfilled
Celanese Hostaform® C 27021 XAP² ™ POM, Unfilled
Celanese Hostaform® C 27021 XAP2® LS POM, UV Resistant
Celanese Hostaform® C 27021 TF POM, Tribological

PHCS327 / 123742

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.