Key Features: 30% Glass Fiber Applications: Automotive: Head Lamp, Tall Lamp, Front Ends Electrical/Electronic: Switches, LED Diffuser Dome & Batten, Energy Meter Housings, Sockets, Relay Case, Connectors Industrial/Household: Industrial Bobbins, Distribution Board Box, Gears & Cams, Power Tool components Information provided by KLJ Group |