MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® MonoPlus SR 7 Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus SR 7 is a macroporous, polystyrene base, monodisperse, nitrate selective anion exchange resin. Lewatit MonoPlus SR 7 has three times the selectivity for nitrates of any commercially available anion exchange resin, which enables it to remove nitrates from sulfate-bearing waters without the danger of nitrate dumping. Dumping occurs in other resins when the nitrate capacity is exhausted and sulfate ions push nitrate ions off the active sites. When this occurs, the effluent with contain more nitrate than the influent. Lewatit MonoPlus SR 7 is ideal for small municipal systems and residential point-of-entry and point-of-use cartridges, because these have a tendency to be overrun and cause nitrates to be dumped. Lewatit MonoPlus SR 7 has been specially prepared to meet drinking water standards and has passed taste and odor tests. Leatit MonoPlus SR 7 is especially suitable for the following applications:
  • the removal of nitrate from drinking water
  • the removal of nitrate from waste water
  • the removal of nitrate from aquarium and fish farming water
  • the removal of nitrate from water
  • the removal of iodide from water
  • the removal of chlorate from concentrated NaOH

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.630 g/cc
Density 1.02 g/cc
Bead Size 0.570 - 0.670 mmMean
Storage Temperature -20.0 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceWhite, opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8805 / 209197

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.