MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ FR C6600 PC+ABS (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY C6600 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable non chlorinated/brominated flame retardant grade with balanced flow, impact and hydrolytic stability. It also offers good chemical resistance and colorability in opaque colors. It has a UL94 V0@1.5mm and 5VB@2.0mm flame rating.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Water Absorption 0.60 %23°C/sat; ISO 62
Moisture Absorption 0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cmSABIC method
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 122ISO 2039-2
Ball Indentation Hardness 110 MPaISO 2039-1
Tensile Strength at Break 50.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa50 mm/min; ISO 527
Elongation at Break >= 50 %50mm/min; ISO 527
Elongation at Yield 4.0 %50 mm/min; ISO 527
Tensile Modulus 2700 MPa1mm/min; ISO 527
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
Flexural Modulus 2700 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
 2.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 25.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 35.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.0040
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 - 400 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KISO 8302
Hot Ball Pressure Test 75.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 95.0 °CRate B/50; ISO 306
 107 °CRate B/120; ISO 306
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 70.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-2
@Thickness 0.750 mm
UL 94
 V-0
@Thickness 1.50 mm
UL 94
 5VB
@Thickness 2.00 mm
UL 94
Oxygen Index 32 %ISO 4589
Glow Wire Test 775 °C
@Thickness 1.00 mm
IEC 60695-2-13
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 250 - 270 °CInjection Molding
Zone 1 230 - 250 °C
Zone 2 240 - 260 °C
Zone 3 250 - 270 °C
Melt Temperature 250 - 270 °C
Mold Temperature 70.0 - 85.0 °C
Drying Temperature 80.0 - 90.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10787 / 244254

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.