MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® E51HSB NC010 PA66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Unreinforced, Heat Stabilized, High Viscosity Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDAM; ISO 1183
Melt Density 0.980 g/cc
@Temperature 295 °C
Water Absorption 8.5 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 2.60 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Number 310 cm³/g90% formic acid; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.013 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.013 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.0 MPa50% RH; ISO 527-1/-2
 84.0 MPaDAM; ISO 527-1/-2
Elongation at Break 35 %Nominal; DAM; ISO 527-1/-2
Elongation at Yield 4.3 %DAM; ISO 527-1/-2
 29 %50% RH; ISO 527-1/-2
Tensile Modulus 1200 MPa50% RH; ISO 527-1/-2
 3100 MPaDAM; ISO 527-1/-2
Flexural Strength 95.0 MPa
@Strain 3.5 %
DAM; ISO 178
Flexural Modulus 2800 MPaDAM; ISO 178
Poissons Ratio 0.37DAM
 0.4450% RH
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 7.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 21.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm50% RH; IEC 62631-3-1
 >= 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Comparative Tracking Index 600 VDAM; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°CDAM; ISO 11359-1/-2
Specific Heat Capacity 2.79 J/g-°C
@Temperature 295 °C
Melt
Thermal Conductivity 0.160 W/m-K
@Temperature 295 °C
Melt
Melting Point 262 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CDAM; ISO 75-1/-2
Vicat Softening Point 221 °C50°C/h, 50N; DAM; ISO 306
Glass Transition Temp, Tg 20.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 70.0 °C10°C/min; DAM; ISO 11357-1/-2
Oxygen Index 20 %DAM; ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 285 °COptimum, Extrusion
 280 - 290 °CRange, Extrusion
 290 - 300 °COptimum, Injection
 290 - 300 °CRange, Injection
Mold Temperature 70.0 °COptimum, Injection
 50.0 - 90.0 °CInjection
Ejection Temperature 190 °CInjection
Drying Temperature 80.0 °CInjection
 80.0 °CExtrusion
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
 4.00 - 6.00 hourExtrusion, Dehumidified Dryer
Moisture Content <= 0.050 %Extrusion
 <= 0.050 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
FMVSS ClassDNIISO 3795 (FMVSS 302)
ISO designationISO 16396-PA66,,M1G1HNR,S32-030
Max. screw tangential speed (m/s)0.4Injection
Part Marking Code>PA66<ISO 11469
PolymerPA66
Processing Hold Pressure Time (s/mm)4Injection
Resin IdentificationPA66ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 150 NC010 POM
Celanese Zytel® ST7301 NC010 PA6-HI
Celanese Minlon® 73M30 NC010 PA6-MD30
Celanese Zytel® 70G35HSLRA4 BK267 PA66-GF35
Delrin Delrin® 100P NC010 POM

PDSX5391 / 198031

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.