MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Toyobo Celanex® 3315-08 PBT, 30% Fiberglass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Product Description: This is a preliminary data sheet. Celanex 3315-08 is a flame retarded, 30% fiberglass reinforced PBT which has an excellent balance of mechanical properties and processability. It is well suited for electrical connector applications. .

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber

Additive: Flame Retardant; Lubricant

Features: Flame Retardant; Lubricated

Forms: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.63 g/ccISO 1183
Water Absorption at Saturation 0.30 %ISO 62
Maximum Moisture Content 0.020
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 20000 psiISO 527-2/5
Elongation at Break 2.1 %ISO 527-2/5
Flexural Strength 28300 psiISO 178
Flexural Modulus 1.23e+6 psiISO 178
Charpy Impact, Notched 4.00 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+13 ohmIEC 62631-3-2
Dielectric Strength 560 V/milIEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 437 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 419 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 401 °FUnannealed; ISO 75-2/A
Flammability, UL94 V-0
@Thickness 0.787 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 68.0 - 122 °FHopper
 482 - 518 °FHot Runner
Feed Temperature 104 - 140 °FInjection
Rear Barrel Temperature 446 - 482 °F
Middle Barrel Temperature 455 - 482 °F
Front Barrel Temperature 464 - 500 °F
Nozzle Temperature 464 - 518 °F
Melt Temperature 464 - 518 °F
Mold Temperature 104 - 176 °F
Drying Temperature 248 - 266 °F
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6195 / 310888

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.