MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LyondellBasell Hostacom 65F4-2C BLK P23726 Polypropylene with 20% Talc Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Hostacom 65F4-2C BLK P23726conventional melt flow, 1,900 MPa flexural modulus, 20% talc-filled polypropylene homopolymer resin.  It has good impact resistance, dimensional stability, colorability and heat aging performance. Applications: Industrial

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 84
Tensile Strength at Break 29.0 MPa
Tensile Strength, Yield 31.0 MPa
Elongation at Break 70 %
Elongation at Yield 4.0 %
Flexural Modulus 1900 MPa
Izod Impact, Notched (ISO) 37.0 kJ/m²
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 109 °Cunannealed
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQT7643 / 219280

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.