MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen GM 5010 T3 BLACK High Density Polyethylene (HDPE), Pipe Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Hostalen GM 5010 T3 black is a high density polyethylene (HDPE), black colored similar RAL 9004 with high melt viscosity for extrusion, injection and compression molding. The product is classified as PE 80 and provides excellent stress crack resistance properties (ESCR) combined with very good long term hydrostatic strength. Applications: Drinking Water Pipe, Gas Pipe, Industrial, Soil & Waste Pipe

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.957 g/ccISO 1183-1
Oxidative Induction Time (OIT) 30 min
@Temperature 210 °C
ISO 11357-6
Carbon Black Loading 2.25 %ISO 6964
Melt Flow 0.43 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 9.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59
@Time 3.00 sec
ISO 868
Tensile Strength, Yield 22.0 MPa50mm/min; ISO 527-1,-2
Elongation at Break >= 350 %ISO 527-1,-2
Elongation at Yield 8.0 %50mm/min; ISO 527-1,-2
Tensile Modulus 1050 MPaISO 527-1,-2
Flexural Modulus 300 MPacreep, 4 point loading/ 2000 hr; DIN 16841
 470 MPacreep, 4 point loading/ 24 hr; DIN 16841
 1000 MPacreep, 4 point loading/1 min; DIN 16841
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -30.0 °C
ISO 179-1/1eA
 24.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eA
Tensile Creep Modulus, 1 hour 640 MPa
@Pressure 2.00 MPa
ISO 899-1
Tensile Creep Modulus, 1000 hours 300 MPa
@Pressure 2.00 MPa
ISO 899-1
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 70.0 °CB50; ISO 306
DSC Induction Temperature 129 °CDSC
 
Descriptive Properties
FNCT (hrs)>100ISO 16770, 4.0 MPa, 2% Arkopal N100, 80°C
MRS Classification (MPA)8ISO 9080
Odor Threshold<=2, EN 1622/EN 1420, measured on pellets/30°C/4 h extraction time
Processing Methodcompression molding, pipe, sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos K38-20-138 Pipe Extrusion Grade Polyethylene
Formosa Plastics Formolene® HP4306 Pipe HDPE
LyondellBasell Hostalen CRP 100 S YELLOW High Density Polyethylene (HDPE), Pipe Grade
Kazanorgsintez PE2NT 11-9 High Density Polyethylene Composite
Kazanorgsintez PE2NT 11-285D High Density Polyethylene Composite

PEQT8490 / 220125

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.