MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ChevronTexaco Hydraulic Safety Fluid
Categories: Fluid; Lubricant

Material Notes: Texaco Hydraulic Safety Fluid is a fire-resistant fluid designed for use in high pressure hydraulic systems where the requirements for fire resistance, pump wear protection and viscosity are satisfied by water-glycol fluids.

Texaco Hydraulic Safety Fluid is a water solution of diethylene glycol containing antiwear agents and rust inhibitors.

Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  • Only distilled or deionized water should be used as makeup. The use of hard tap water, well or spring water should be avoided since the dissolved minerals in these waters will react with the additive system in the fluid to cause fluid haziness and formation of soap-like insoluble material.

    Fluid with a viscosity below 36.2 cSt at 40°C, or Brix readings below 42, contain excess water and only new Texaco Hydraulic Safety Fluid should be used as makeup.

CPS Number: 220766; MSDS Number: 10587

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity -1.70 °
Viscosity Measurement 201Viscosity Index
Saybolt Viscosity at 100°F 227 SUS
Saybolt Viscosity at 210°F 55.7 SUS
Kinematic Viscosity at 40°C (104°F) 41 cSt
Kinematic Viscosity at 100°C (212°F) 8.8 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -74.0 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content 40 %vol% after makeup
 
Descriptive Properties
Brix Number42-44.538.5 - 41.4% H2O
 4537.7% H2O, 2 gal. adjustment, See Notes 1, 2
 4636.3% H2O, 4 gal. adjustment, See Notes 1, 2
 4734.7% H2O, 7 gal. adjustment, See Notes 1, 2
 4833.3% H2O, 10 gal. adjustment, See Notes 1, 2
 4931.7% H2O, 12 gal. adjustment, See Notes 1, 2
 5030.3% H2O, 14 gal. adjustment, See Notes 1, 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WTEXA095 / 76974

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.