Westlake 2060 is a low molecular weight, film and medical grade, vinyl suspension resin. Designed for clear and opaque, rigid injection and blow molding applications. This resin has good clarity, color and thermal stability. Kosher approved. Applications: suited for high flow injection and blow molding products.Information provided by Westlake Chemical. |