Europrene Latice® B 010 is an aqueous anionic dispersion of a styrene-butadiene copolymer with medium solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain any antioxidant. Key Features: Europrene Latice® B 010 is mainly blended with other styrene-butadiene lattices or natural latex to increase stiffness. Main Applications: Europrene Latice® 5570 is used as a reinforcing latex. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |