Production Method: Obtained by interaction of ethylene oxide with polyethyleneglycol-9 is presence of catalyst. Application: Polyethyleneglycol-68 finds its application in production of man-made fibers as a modifier, in particular for production of high-strength viscose cords. Information Provided by Kazanorgsintez |