MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Envalior Pocan® DP 7244 000000 PBT, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: PBT, 30% glass fibers, injection molding, flame retardant

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/ccISO 1183
Water Absorption 0.40 %Test Sim. to ISO 62
Moisture Absorption at Equilibrium 0.20 %23°C/50% R.H.; Test Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4, 2577
Melt Flow 31 g/10 min
@Load 2.16 kg,
Temperature 260 °C
Estimated using room temperature density; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 145 MPaISO 527-1/-2
Elongation at Break 2.5 %ISO 527-1/-2
 3.0 %Nominal; ISO 527-1/-2
Tensile Modulus 11000 MPaISO 527-1/-2
Charpy Impact Unnotched 55.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 200 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 223 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 150 °CISO 75-1/-2
Flammability, UL94 V-0
@Thickness 0.750 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection Molding; ISO 294
Mold Temperature 80.0 °CInjection Molding; ISO 10724
 
Descriptive Properties
AdditivesFlame retarding agent
 Release agent
FeaturesFlame retardant
FormPellets
ISO Short NameISO 7792-1-PBT,GFR,07-110,GF30; ISO 1043-PBT GF FR(17)
ProcessingInjection molding
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Arnite® TV4 240 S PBT-20% Glass Reinforced (European and Asian Grade)
Envalior Pocan® DP 4035 000000 PBT, 30% Glass Fiber Reinforced
Envalior Pocan® KU 2-7604 000000 PBT+PC
Envalior Pocan® BF 4222 000000 PBT, 20% Glass Fiber Reinforced
Envalior Pocan® B 3235 000000 PBT, 30% Glass Fiber

PLANX0881 / 99096

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.