VORANOL™ CP 6001 polyol is a triol polyether polyol, capped, specially developed for the production flexible HR molded polyurethane foam with TDI, TDI/PMDI or MDI. It can be used in the production of semi-rigid integral skin foams as well as in the production of cold cure molded foams and high resilience molded. Information provided by Dow |