MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Glyptal 2600 Alkyd Nitrocellulose Lacquer
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: GLYPTAL 2600 Gloss Black Lacquer was designed or general purpose finishing of industrial products. This alkyd nitrocellulose lacquer has excellent weather durability and very good arc resistance and dielectric strength.

SUGGESTED USES

GLYPTAL 2600 can be used where a fast, air-drying finish is desired. Because of its excellent weather durability, this lacquer may be used on exterior surfaces as well as interior surfaces. Electrical equipment, instruments, and switchboards can be coated with this lacquer as well as furniture, toys, and office equipment.

APPLICATION

GLYPTAL 2600 may be applied by spray or dip methods. When used to finish metal surfaces, it is preferable that a primer such as Glyptal 7920 be used first.

REDUCTION

For spray or dip application, thin 2600 Black Lacquer with approximately equal volume of G1514 Lacquer Thinner to 20-25 seconds #2 Zahn Cup.

SURFACE PREPARATION

Surfaces to be painted should be dry and free from dirt, wax, grease, rust, and oil. Remove grease and oil by washing surface with mineral spirits. Allow surface to dry thoroughly. When painting over a glossy surface, reduce gloss by using fine sand paper or steel wool.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Flash Point <= 80.0 °F
 
Processing PropertiesOriginal ValueComments
Dry Time 0.500 hourAir Dry: Touch
 4.00 hourAir Dry: Hard
 
Descriptive Properties
ColorBlack
Coverage350 ft²/gal1 mil dried film
GlossHigh
RecoatOvernight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Michelman® Micryl™ 766R Water resistant coating
KaMin Hydrasperse® Kaolin Clay - Filler
KaMin Hydramatte® Kaolin Clay - Filler
KaMin Hydragloss® 90 Clay
KaMin Hydrafine® Clay

PGLYPT911 / 209750

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.