MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ExxonMobil ExxonMobil™ PP1352E1 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: A medium melt flow rate homopolymer resin designed  for appliance and other consumer products requiring long-term heat aging resistance.

Availability:  North America.  Features:  detergent resistant, heat aging resistant, thermal aging resistant, general purpose, heat stabilized, good processability, medium flow.  Applications: appliance components, appliances, consumer applications.   Appearance:  natural color.  Forms: pellets.  Processing Method:  compounding, extrusion, injection molding.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccExxonMobil Method
Melt Flow 5.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 5240 psi2.0 in/min; ASTM D638
Elongation at Yield 10 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 224000 psi0.051 in/min; ASTM D790A
 255000 psi0.51 in/min; ASTM D790B
Izod Impact, Notched 0.660 ft-lb/in
@Temperature 22.8 °C
ASTM D 256A
Izod Impact, Unnotched 0.400 ft-lb/in
@Temperature -17.8 °C
ASTM D256E
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 200 °Funannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °Funannealed; ASTM D648
 
Descriptive Properties
Rockwell Hardness101ASTM D785

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX98981 / 238362

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.