System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Multibase Multi-Pro® 0112 Black Polypropylene
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Molded
Material Notes:
Multi-Pro 0112 is a nucleated and antistated polypropylene homopolymer. It is designed for injection molding applications that require superior mold release properties.
Data provided by Multibase.
Key Words:
PP
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.900
g/cc
ASTM D792-91
Melt Flow
12
g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D-1238-94a
Mechanical Properties
Original Value
Comments
Hardness, Shore D
76
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate
31.0
MPa
ASTM D638-95
Tensile Strength, Yield
34.5
MPa
ASTM D638-95
Elongation at Break
570 %
ASTM D638-95
Elongation at Yield
10 %
ASTM D638-95
Tensile Modulus
1.52
GPa
Secant at 1% strain; ASTM D-638-95
Flexural Modulus, 1% Secant
1.241
GPa
ASTM D-790-95
Izod Impact, Notched
0.270
J/cm
ASTM D256-93a
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
RTP Company ESD A 100 HF Polypropylene (PP); ESD Protection - Static Dissipative
Premix Thermoplastics PRE-ELEC® PP 1370
Inno-Comp INNOPOL® CS 2-3000 Polypropylene Block-Copolymer
Ineos N12N-00 Polypropylene Impact Copolymer
Ineos H12F-00 Polypropylene Homopolymer
PLA242 / 49639
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.