MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound WX05502 Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP THERMOCOMP WX05502 compound is based on Polybutylene Terephthalate (PBT) resin containing 45% glass fiber/mineral. Added features of this grade include: Flame Retardant.

Features: Flame Retardant,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.81 g/ccASTM D792
Density 1.80 g/ccASTM D792
Moisture Absorption 0.0200 %23°C/50% RH/24 hrs; ASTM D570
 0.0200 %Injection Molding
 0.0300 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.030 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 85.0 MPa5 mm/min; ISO 527
 90.0 MPa5 mm/min; ASTM D638
Elongation at Break 1.2 %5 mm/min; ISO 527
 1.4 %5 mm/min; ASTM D638
Elongation at Yield 1.2 %5 mm/min; ISO 527
Tensile Modulus 11740 MPa1 mm/min; ISO 527
 13240 MPa50 mm/min; ASTM D638
Flexural Strength 141 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 142 MPaISO 178
Flexural Modulus 10900 MPa1.3 mm/min, 50 mm span; ASTM D790
 11380 MPa2 mm/min; ISO 178
Izod Impact Notched 18.0 JASTM D256
Izod Impact, Unnotched 337 J/mASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 22.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 8.00 JASTM D3763
Impact Test 1.00 JMultiaxial Impact; ISO 6603
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=0.750 mm
UL 746A
 30 - 60 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
@Thickness >=3.00 mm
UL 746A
 30 - 60 arcs
@Thickness >=1.50 mm
UL 746A
 >= 120 arcs
@Thickness >=0.750 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 217 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 221 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 197 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 205 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 130 °CUL 746B
UL RTI, Mechanical without Impact 140 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.750 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 250 - 260 °C
Zone 3 265 - 275 °C
Melt Temperature 250 - 275 °CInjection Molding
Mold Temperature 80.0 - 95.0 °C
Drying Temperature 120 - 150 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF2UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81964 / 289911

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.