MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI KYDEX® V103 Thermoplastic
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic

Material Notes: High impact fire-rated sheet

KYDEX® V103 sheet is a recycled grade of a proprietary thermoplastic sheet that is cost competitive with other grades of thermoplastic sheet while offering improved performance.

KYDEX® V103 is Underwriters Laboratories, Inc® recognized Std 94 V-0, 5V. It has thermoforming cycle times equivalent to FR-ABS.

Suggested Applications:

  • Equipment Housings
  • Exhibits and Displays
  • Miscellaneous Applications

Features:

  • Formulated to substitute for FR-ABS
  • Very good impact resistance
  • Easy to form with excellent part definition and deep-draw characteristics
  • Recognized by Underwriters Laboratories, Inc® for Std 94 V-0, 5V
  • Similar forming times to FR-ABS
  • Available in 7 distinctive textures

Values based upon 3.18 mm (0.125 in) sheet unless otherwise specified.

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 94ASTM D785
Tensile Strength 41.0 MPaASTM D638
Modulus of Elasticity 2.48 GPaASTM D790
Flexural Strength 65.5 MPaASTM D790
Izod Impact, Notched 427 J/m
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 165 °FAnnealed; ASTM D648
Flammability, UL94 V-0UL File E115252; Component Recognition
 5VB
@Thickness >=0.711 mm
Underwriters Laboratories, Inc®, File E115252; Component Recognition; UL Standard 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® 410 ABS/PVC
SEKISUI SPI KYDEX® 430 ABS/PVC
SEKISUI SPI KYDEX® 6513 Thermoplastic
SEKISUI SPI KYDEX® 110 Polymer Alloy Sheet
SEKISUI SPI KYDEX® 100 Polymer Alloy Sheet

PSEKIS049 / 185874

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.