MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Celanese Celanex® MT2008 PBT, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Density 1.31 g/ccISO 1183
Water Absorption 0.090 %
@Temperature 22.8 °C
24hr immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cmASTM D955
 0.018 - 0.020 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 72ISO 2039-2
Tensile Strength at Break 60.0 MPa5mm/min; ISO 527-2/1A
Tensile Strength, Yield 8000 psiASTM D638
Elongation at Break 5.0 %5mm/min; ISO 527-2/1A
 5.0 %ASTM D638
Flexural Strength 80.0 MPaISO 178
 12000 psiASTM D790
Flexural Modulus 2200 MPaISO 178
 330000 psiASTM D790
Izod Impact, Notched 0.500 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 3.10 kJ/m²ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
ASTM D150
 3.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 15.0 kV/mmIEC 60243-1
 400 V/milshort term; ASTM D149
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
ASTM D150
 0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °C10°C/min; ISO 11357-1,-2,-3
 437 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 155 °CISO 75-1, -2
 310 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °CISO 75-1, -2
 130 °FASTM D648
Glass Transition Temp, Tg 60.0 °CISO 11357-1,-2,-3
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 65.0 - 93.0 °Ccavity
 250 - 260 °Chot runner
Feed Temperature 230 - 240 °C
Zone 1 230 - 240 °C
Zone 2 235 - 250 °C
Zone 3 235 - 250 °C
Zone 4 240 - 260 °C
Die Temperature 250 - 260 °C
Melt Temperature 243 °CISO 294
 235 - 260 °C
Mold Temperature 82.0 °CISO 294
Injection Velocity 300 mm/secISO 294
Drying Temperature 120 - 130 °C
Dry Time 4.00 hour
Moisture Content <= 0.020 %
Hold Pressure 48.0 MPaISO 294
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing conditions acc. ISO7792-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celanex® 2401 MT PBT, Medical Technology
Celanese Celanex® 2300 GV1/10 PBT, 10% Glass Reinforced
Celanese Celanex® 2008 PBT, Unfilled
Celanese Celanex® 2003HR PBT, Unfilled
Celanese Celanex® 2002-3 PBT, Unfilled

PHCQ093 / 178548

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.