MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Petroquimica Triunfo Trithene® TS 8090 MDPE - Thermal Shrink Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: The Trithene TS 8090 resin is a medium-density polyethylene (MDPE) with a high molecular weight that presents excellent mechanical resistance, along with good optical properties and increased stiffness. These characteristics ensure the production of a packaging with a good appearance, low level of breakage, and elevated support structure during manual transport (the film remains firm even when picked up by the edges). The Trithene TS 8090 resin presents flow properties than ensure an excellent processability with conventional extruders for LDPE, granting low energy consumption during the whole process and allowing for the production of films with a good dimensional uniformity and an excellent surface finishing. The incorporated additives package warrants thermal stability during processing, low coefficient of friction (COF), and low static, which are indispensable for high productivity on the printing, cutting and welding, and shrink-wrap lines. This product complies with ASTM standard D1248-IIA5 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.

Applications: Technical shrink-wrap films for unitization of various products such as soft drink and mineral water bottles, soft drink cans, beers, paints, etc. Monolayer and multi-layer technical films.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Petroquimica Triunfo has been acquired by Braskem.

Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.928 - 0.930 g/ccASTM D1505
Thickness 50.0 microns
Melt Index of Compound 0.12 - 0.16 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 19.0 MPaASTM D638
Tensile Strength, Yield 13.5 MPaASTM D638
Film Elongation at Break, MD 250 %ASTM D882
Film Elongation at Break, TD 625 %ASTM D882
Elongation at Break 600 %ASTM D638
Secant Modulus, MD 0.148 GPa5%; ASTM D882
Secant Modulus, TD 0.163 GPa5%; ASTM D882
Coefficient of Friction, Dynamic 0.13ASTM D1894
Elmendorf Tear Strength, MD 5.60 g/micronASTM D1922
Elmendorf Tear Strength, TD 5.00 g/micronASTM D1922
Dart Drop Test 180 g(method A); ASTM D1709
Film Tensile Strength at Break, MD 27.5 MPaASTM D882
Film Tensile Strength at Break, TD 25.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 116 °CASTM D3418
 
Optical PropertiesOriginal ValueComments
Haze 18 %ASTM D1003
Gloss 60 %@ 60° Gardner; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 175 °CPlasticizing Zone
 170 - 185 °CMixture Zone
Feed Temperature 150 - 165 °C
Adapter Temperature 180 - 195 °C
Die Opening 0.00350 - 0.0200 cm
Blow-up Ratio (BUR) 3.0Or Greater
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum Weldalite 049-T6
Aluminum Weldalite 049-T4
Aluminum Weldalite 049-Reversion
Aluminum 8090-T8x
Aluminum 8090-T8771 and 8090-T651

PDAX104 / 29529

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.