Universal 316 is a chromium-nickel alloy with large amounts of molybdenum added for superior corrosion resistance and strength. The corrosion resistance is superior to types 302 and 304 making 316 the choice for those applications requiring superior creep strength and corrosion resistance. Information provided by Universal Wire Works for their line of welding wire and filler metal. |