MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
VICTREX HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliant, colour natural/beige.

Typical Application Areas:

Higher temperature applications where higher strength in a static system is required. Low coefficient of thermal expansion. Chemically resistant to aggressive environments, suitable for sterilization for medical and food contact applications.

Information Provided by Victrex.

Key Words: PEK
Vendors: With over 30 years of focus, experience and security of supply Victrex Polymer Solutions is the world’s leading manufacturer of high performance Polyaryletherketones (PAEK) including versatile VICTREX™ PEEK. We work with our customers and end users to deliver technology driven solutions to meet the challenges and opportunities they face and help them to achieve new levels of cost savings, quality and performance. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.53 g/ccCrystalline; ISO 1183
Water Absorption at Saturation 0.50 %
@Temperature 23.0 °C
ISO 62-1
 0.60 %
@Temperature 100 °C
ISO 62-1
Viscosity 450000 cP
@Temperature 400 °C
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0030 cm/cm395°C nozzle, 200°C tool; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm395°C nozzle, 200°C tool; ISO 294-4
Spiral Flow 10.5 cm
@Thickness 1.00 mm
Mold Temp: 200°C, Melt Temp: 395°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88
@Temperature 23.0 °C
ISO 868
Tensile Strength at Break 55.0 MPa
@Temperature 275 °C
ISO 527
 65.0 MPa
@Temperature 225 °C
ISO 527
 75.0 MPa
@Temperature 175 °C
ISO 527
 125 MPa
@Temperature 125 °C
ISO 527
 200 MPa
@Temperature 23.0 °C
ISO 527
Elongation at Break 2.9 %
@Temperature 23.0 °C
ISO 527
Tensile Modulus 12.0 GPa
@Temperature 23.0 °C
ISO 527
Flexural Strength 85.0 MPa
@Temperature 275 °C
ISO 178
 120 MPa
@Temperature 175 °C
ISO 178
 210 MPa
@Temperature 123 °C
ISO 178
 290 MPa
@Temperature 23.0 °C
ISO 178
Flexural Modulus 11.0 GPa
@Temperature 23.0 °C
ISO 178
Compressive Strength 50.0 MPa
@Temperature 250 °C
ISO 604
 75.0 MPa
@Temperature 200 °C
ISO 604
 180 MPa
@Temperature 120 °C
ISO 604
 290 MPa
@Temperature 23.0 °C
ISO 604
Izod Impact, Notched (ISO) 11.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Izod Impact, Unnotched (ISO) 70.0 kJ/m²
@Temperature 23.0 °C
ISO 180/U
Charpy Impact Unnotched 7.00 J/cm²
@Temperature 23.0 °C
SO 179/1U
Charpy Impact, Notched 0.900 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Dielectric Constant 3.2
@Frequency 1000 Hz,
Temperature 23.0 °C
IEC 60250
Dielectric Strength 23.0 kV/mm
@Thickness 2.00 mm
IEC 60243-1
Dissipation Factor 0.0050
@Frequency 1e+6 Hz,
Temperature 23.0 °C
IEC 60250
Comparative Tracking Index 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature <=152 °C
Below Tg; ISO 11359
 25.0 µm/m-°C
@Temperature >=152 °C
Above Tg; ISO 11359
CTE, linear, Transverse to Flow 45.0 µm/m-°C
@Temperature <=152 °C
Below Tg; ISO 11359
 110 µm/m-°C
@Temperature >=153 °C
Above Tg; ISO 11359
Thermal Conductivity 0.300 W/m-K
@Temperature 23.0 °C
Average; ISO/CD 22007-4
 0.350 W/m-K
@Temperature 23.0 °C
Along flow; ISO 22007-4
Melting Point 373 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 360 °CISO 75-f
Glass Transition Temp, Tg 152 °COnset; ISO 11357
 160 °CMidpoint; ISO 11357
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 100 °CHopper Temperature
Rear Barrel Temperature 375 °C
Middle Barrel Temperature 380 - 385 °C
Front Barrel Temperature 390 °C
Nozzle Temperature 395 °C
Mold Temperature 190 - 215 °C
Drying Temperature 120 - 150 °C
Dry Time 3.00 - 5.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450CA30 30% Carbon Fiber Reinforced
VICTREX™ PEEK 450GL30 30% Glass Fiber Reinforced
VICTREX™ PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
VICTREX™ PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced
VICTREX ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced

PVICTA56 / 99734

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.