MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Mikro-Technik DT R Carboxymethylcellulose (CMC)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic

Material Notes: Purified Grade. Custom formulations are available.
  • All grades are available neutralized with carbon dioxide (no suffix or suffix K) or acetic acid (suffix E).
  • Reduced active contents down to 50% are available.
  • Most of the grades are available as powder or granules.
  • The viscosity listed is typical.

Information provided by Mikro-Technik GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 5.0 - 15 cP
@Temperature 20.0 °C
2%, Hoppler
 
Descriptive Properties
Degree of Substitution0.75
Max. Active Content %, on dry basis98

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cotronics Duralco™ 125 450°F Stress Free, Silver Filled Epoxy, Thermally Conductive
Dow HV 1520/40
Dow HS III HS SPRAYABLE CATALYST - CLEAR
CHT Group QSil 553 QSI Quantum Silicones Silicone Potting Material
CHT Group QSil 40 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting

PMIKROT12 / 53111

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.