MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
CMT Materials REN Shape® 470 Tooling Board, Modeling Board, Adhesive Products
Categories: Polymer

Material Notes: CMT Materials offers the complete line of REN Shape tooling board, modeling board, and related adhesive products. Vacuum formers and thermoformers use these products as prototype and low volume production molds when forming in applications where metal molds do not makes sense due to time or cost considerations. CMT can help in selecting the proper board material for specific forming applications considering factors such as surface quality, ease in machining, tool durability, and forming temperature.

Information Provided by CMT Materials, Inc.

Key Words: Renshape
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 104 lb/ft³ASTM D-792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90ASTM D-2240
Tensile Strength, Ultimate 4700 psiASTM D-638
Flexural Strength 8700 psiASTM D-790
Flexural Modulus 983 ksiASTM D-790
Compressive Strength 9500 psiASTM D-695
Compressive Modulus 866 ksiASTM D-695
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.7 µin/in-°FASTM D-3386
Glass Transition Temp, Tg 232 °FASTM D-4065
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCMT016 / 93165

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.