MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Oboto Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Mechanical properties reported according to ASTM D143 at 12 wt% moisture content.

Key Words: Mammea africana, timber, lumber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.530 - 0.700 g/ccOven-dry to green volume ratio
Density 0.657 - 0.865 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 14.34 - 14.62 GPa
Modulus of Rupture 0.13858 - 0.16065 GPa
Compressive Strength 68.26 - 77.22 MPaparallel
 
Thermal PropertiesOriginal ValueComments
Shrinkage 6.5 %radial; from green to oven-dry condition based on initial condition when green
 10 %tangent
 
Descriptive Properties
CategoryHardwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Assab Steels ASSAB XW-41 Cold Work Steel
North American Loblolly Pine Wood
North American Western Larch Wood
North American White Fir Wood
Northern White Pine Wood

PTSU074 / 100543

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.