MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Marco Polo MARPOL LDF 723-B Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: MARPOL® LDF 723-B is a medium density homopolymer film resin with good clarity and excellent stiffness. Films made from this resin are designed for overwrap applications and push-through type packaging. It is suitable for processing in either blown or cast film equipment.

Recommended Applications: Bread bags, cast film, co-extrusion films, diaper backsheet, hygiene packaging, label film, overwrap film, paper overwrap..

Additives: Slip – 1000 ppm; Antiblock – no.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.929 g/ccASTM D1505
Melt Flow 2.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Slip Level 1000 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 2100 psiASTM D882
Film Tensile Strength at Yield, TD 2300 psiASTM D882
Film Elongation at Break, MD 180 %ASTM D882
Film Elongation at Break, TD 460 %ASTM D882
1% Secant Modulus 47000 psiMD; ASTM D882
 56000 psiTD; ASTM D882
Elmendorf Tear Strength MD 100 gASTM D1922
Elmendorf Tear Strength TD 270 gASTM D1922
Dart Drop Test 70.0 gASTM D1709
Film Tensile Strength at Break, MD 3400 psiASTM D882
Film Tensile Strength at Break, TD 2500 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 117 °CPeak; ASTM D3418
 
Optical PropertiesOriginal ValueComments
Haze 8.1 %ASTM D1003
Gloss 68 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMARCO102 / 283699

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.