MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Titanium (IV) Oxide, TiO2
Categories: Ceramic; Oxide

Material Notes: CAS Number: 13463-67-7

Physical Form: White Tetragonal Crystals

MatWeb has separate entries for different forms of TiO2, including rutile, anatase, and brookite.

Key Words: TiO2, Titanium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.23 g/cc
Molecular Weight 79.866 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 5.8
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.6887 J/g-°CCrystal
Melting Point 1843 °C
Heat of Formation -944 kJ/molCrystal
 
Optical PropertiesOriginal ValueComments
Refractive Index 2.538na
 2.584nß
 2.70
@Wavelength 435.8 nm
ng
 
Descriptive Properties
SolubilityInsoluble in H2O and diluted Acid; Soluble in concentrated Acid
SynonymBrookite

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Dioxide, Rutile
Titanium Dioxide, Brookite
Titanium Dioxide, TiO2, Anatase
Titanium (IV) Sulfide, TiS2
Zirconium Oxide, Zirconia, ZrO2

EINOR3299 / 5387

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.