MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Freudenberg Simriz® 489 Ultra Pure FFKT Perfluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of elasticity. Simriz® perfluoro elastomers close the material gap between inelastic PTFE and elastomers, which have poor temperature and chemical resistance properties. With a fluoridation level of 72%, FFKM elastomers have a level of resistance close to that of pure PTFE at 76%. At the same time, FFKM materials are so elastic that they are excellently suited to both static and dynamic seals. Simrit offers ISC O-Rings which are specifically optimised with respect to flexibility at low temperatures, resistance to high temperatures, hardness, tensile strength, elongation, compression set, or color.

Information provided by Freudenburg-NOK.

This product was formerly sold under the Freudenberg Simrit division; now Freudenberg Sealing Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 69ASTM D2240
Tensile Strength 13.5 MPaASTM D1414
Elongation at Break 235 %ASTM D1414
100% Modulus 2.70 MPaASTM D1414
Compression Set 25 %
@Temperature 250 °C,
Time 252000 sec
ASTM D395 Method B
 28 %
@Temperature 250 °C,
Time 252000 sec
ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °C
Minimum Service Temperature, Air 0.000 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Manufacturer specifies transparent but does not quantify
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Freudenberg Simriz® 481 Low Temperature FFKT Perfluoroelastomer Compound
Freudenberg Simriz® 483 Low Temperature FFKT Perfluoroelastomer Compound
Precision Polymer Engineering Perlast® G67P Translucent Perfluoroelastomer
Daikin DAI-EL® Perfluor GA-15 Perfluoroelastomer
DuPont Mobility and Materials Kalrez® AeroSeal™ 7797 Fluoroelastomer

PSIMR008 / 67732

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.