MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Garlock GYLON® 3500 PTFE Gasketing, Silica Filler
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: PTFE with silica filler.
  • Improved sealing performance over conventional PTFE
  • Unique manufacturing process minimizes cold flow problems typical of skived and expanded PTFE sheets
  • Excellent bolt torque retention
  • Withstands a wide range of chemicals for extended service life
Media: Strong acids (except hydrofluoric), Solvents, Hydrocarbons, Water, Steam, Chlorine, Cryogenics

Information provided by Garlock Rubber Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Permeability 0.015Gas Permeability, cc/min; DIN 3535 Part 4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2000 psiacross grain; ASTM F152
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 362 V/mil
@Temperature 121 °C,
Time 10800 sec
0.0625 in. thickness; ASTM D149
 61.0 V/mil
@Thickness 1.59 mm
100% RH for 96 hours; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
@Pressure 8.27 MPa
Continuous
Minimum Service Temperature, Air -450 °F
 
Descriptive Properties
ColorFawn
Compressibility, %7-12ASTM F36
Creep Relaxation, %18ASTM F38
Sealability ASTM F37B, ml/hr0.22ASTM Fuel A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Beijing Evergrow Resources PTFE, 20% Glass Fiber, 5% Graphite Filled
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.001" thick)
3M Dyneon™ CC085 PTFE, PPS-Filled
Klinger Thermoseal KLINGERSIL® C-4401 General Application Gasketing
Klinger Thermoseal Klinger® Quantum Hydrogenated Nitrile Butadiene Rubber (HNBR)

PGARL811 / 157491

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.